CERA PLASTER is a Fiber Reinforced, Polymer modified Cement base, Preblended High Strength & Hydrophobic property multipurpose non shrink readymix Plaster. For Plastering internal and external surface of the walls made from A.A.C. Blocks/ Concrete Blocks, Bricks, R.C.C. Stone /Chira surfaces, Ceiling & other Repairing work
Ceraplaster Ready [Mix Plaster can be applied on
- Fired Clay Brick Walls
- Stone Walls
- AAC Block Walls.
- Fly Ash Block Walls.
- Concrete Block Walls.
- Concrete Surfaces.
Packing
50 kg Bags.
Coverage
1 kg will cover approximately 20+- 3 sqft (Depends on the surface).
| Thickness(MM) | 3 | 5 | 10 | 12 | 15 | 18 |
|---|---|---|---|---|---|---|
| Qty required/ Sft (Kg) approximate) |
0.46 | 0.77 | 1.53 | 1.84 | 2.30 | 3.07 |
| Packing / Bag (Kg) | 40.00 | 40.00 | 40.00 | 40.00 | 40.00 | 40.00 |
| Approximate Coverage / Bag(sft) | 86.00 | 52.00 | 15.00 | 21.00 | 17.00 | 13.00 |
How to use
- Material received at site in first lot shall be used first and same practice shall be followed. Do not mix any material in CERA PLASTER Except clean water.In case of mechanical mixer, CERA PLASTER shall be added in 130 140 ml/kg clean water & mix it thoroughly for minimum 3 min and in case of hand mixing. CERAPLAST shall beadded in 150-160 ML per kg clean water as per consistency required as per site condition & it shall be mixed for 8 to 10 minutes. Accordingly for 40 kg bag of CERA PLAST water shall be added in mixing trey/Pot/ mechanical mixer / stirrer and it shall be mix thoroughly till we get the uniform consistency to the
mix material, allow mix material remain idle for 3 to 5 minutes polymer / adhesives / fibres to be dissolved to get the special properties to the plaster. Surface to be plaster shall be made clean, dust & Curing compound free & wet before starting the plastering work. No need to apply any bonding agent on the walls / other surface before Plastering with CERA PLAST. - Again mix the material and check the consistency/ workability of CERA PLAST before starting the plastering work, mix material of plaster shall be applied on all over surfaces by spreading mixed material by tower uniformly to maintain level, thickness and to get the smooth finish / sand face plaster can be done by using sponge.
- In case of normal weather condition, curing shall be done twice in a day after 12 hour at least 2 to 3 days & In case of hot or extreme hot weather curing may done for 5 to 6 days.
Inquiries